dianoir® G3, deposited at a temperature <190ºC, is ideal for coating complex shaped components and delicate materials that cannot be coated with traditional PVD technologies. dianoir® G3 is resistant to chemical products and acidic and alkaline solvents and is hypoallergenic; it is therefore highly valued for coating watch bracelets.

dianoir® G3

Characteristics
Advantages
Download
Technology a-C:H
Process PACVD
Structure Amorphous
sp3 fraction [%] 40-60
Color Black
Thickness 2-3 µm
Deposition temperature [°C]  ≥190
Hardness [GPa] 19-24
Hardness HV 0.05 2000-2500

 

Generic remark: all data are approximate values. These ranges, depending on geometry, substrate, and surface finish, could also vary significantly.

The values shown refer to measurements made on samples in INOX 316.

 

 

 

dianoir®G3, which is particularly suitable for watchmaking components, has the following advantages:
- excellent adhesion on brass, stainless steel and titanium alloy components
homogeneous black color
- decorative and functional coating in one solution
- non-toxic process and biological compatibility are optimal properties for the use of dianoir®G3 in contact with the human skin
- ideal for all watch movement components that will benefit from an improvement in their tribological and decorative properties